高强无收缩水泥灌浆料
项目
|
标准技术指标
|
普通型
|
高强型
|
早强型
|
||
粒径
|
4.75mm方孔筛筛余/%
|
≦2.0
|
≦2.0
|
≦2.0
|
≦2.0
|
|
凝结时间
|
初凝/min
|
≧120
|
≧120
|
≧120
|
≧60
|
|
泌水率/ %
|
≦1.0
|
≦1.0
|
≦1.0
|
≦1.0
|
||
流动度/mm
|
初始流动度
|
≧264
|
≧280
|
≧280
|
≧280
|
|
30min保留值
|
≧240
|
≧260
|
≧260
|
≧260
|
||
抗压强度/MPa
|
6h
|
—
|
—
|
—
|
≧25.0
|
|
1d
|
≧22.0
|
≧25.0
|
≧40.0
|
≧45.0
|
||
3d
|
≧40.0
|
≧45.0
|
≧60.0
|
≧65.0
|
||
28d
|
≧70.0
|
≧75.0
|
≧80.0
|
≧80.0
|
||
竖向膨胀率/ %
|
1d
|
≧0.020
|
≧0.020
|
≧0.020
|
≧0.020
|
|
钢筋握裹强度(圆钢)/MPa
|
28d
|
≧4.0
|
≧6.0
|
≧6.0
|
≧6.0
|
|
对钢筋有无锈蚀作用
|
对钢筋无锈蚀作用
|