名称 | 镍基焊条 | 规格 | 2.5--5.0 |
---|---|---|---|
适用范围 | 不锈钢,耐晶间腐蚀和湿法腐蚀 400°C(752°F)。 |
Thermanit 30/40 EW | 符合 EN ISO 14172 Mat. No. E Ni 8025 (NiCr29Fe30Mo) 2.4653 |
||||||||||
耐晶间腐蚀不锈钢;湿法腐蚀450°C(842°F)。耐腐蚀性能好,特别是在减少环境。(和热裂解的阻力耐腐蚀)Thermanit 30/40电子战优于完全奥氏体X 6 NiCrCuNb 20 18 - 25 X 5 CrNiMoNb 25焊接填充金属、热裂化非常敏感。加入,忽而与匹配和相似,非稳定和稳定完全奥氏体钢/铸钢的成绩含钼(铜)。加入上述钢纯粹的/低合金钢。 Stainless; resistant to intercrystalline corrosion – wet corrosionup to 450 °C (842 °F). Good corrosion resistance, especially inreducing environments. In terms of hot cracking resistance (andcorrosion resistance) Thermanit 30/40 EW is superior to the fullyaustenitic X 6 NiCrCuNb 20 18 and X 5 CrNiMoNb 25 25welding filler metals, which are very sensitive to hot cracking.For joining and surfacing work with matching and similar, nonstabilized and stabilized fullyaustenitic steels/cast steel gradescontaining Mo (and Cu). For joining aforementioned steels tounalloyed/low alloy steels.
|
|||||||||||
|
|||||||||||
熔敷金属化学成分(%)C Si Mn Cr Mo Ni Cu <0.03 <0.9 1.5 28.0 4.3 36.0 1.8 |
|||||||||||
熔敷金属力学性能Heat- Yield strength Yield strength Tensile Elongation Impact values treatment 0.2% 1.0% strength (L0=5d0) in J CVN N/mm2 N/mm2 N/mm2 % AW 350 370 550 30 50 |
|||||||||||
参考电流 (AC、DC+)
|
蒂森焊丝12
蒂森焊条_conew1
蒂森焊丝352
蒂森焊材2_conew1
蒂森焊条7+8+9+6
蒂森焊条7+89
蒂森焊丝9988
蒂森焊丝2288
Tel:
Tel:
Tel:
Tel: