产品编号:TDL-013(外)
Serial Number: TDL-013W
Function: protective mortar for external thermal insulation system
产品介绍:采用目前世界上**先进的三元共聚再分散粉料作为助剂生产的干粉砂浆,改变了传统水泥砂浆机理结构,形成了一个完整的三维网络,具有良好的抗裂性、粘结性、耐候性(耐老化)和防水透汽性。
Product Introduction: the most advanced redispersible powder is used as additive, which changes the composition of traditional mortar and forms a three dimensional net, so the product is anti-crack, adhesive, weatherproofing and waterproof.
技术性能:
项目 |
性能 |
|
拉伸粘接强度(与聚苯板) |
原强度,MPa |
≥ 0.10, 聚苯板破坏 |
耐水强度,MPa |
||
耐冻融强度,MPa |
||
可操作时间, h |
1.5-4.0 |
|
柔韧性(抗压强度/抗折强度) |
≤3.0 |
|
外观 |
单组分,干粉,灰色粉末 |
Technical Specifications:
Items |
Specification |
|
Tensile bond strength (with cement board) |
Primary,MPa |
≥ 0.10, and EPS destructed |
Water-tolerant,MPa |
||
Freezing and thawing bearing,MPa |
||
Work life, h |
1.5-4.0 |
|
Flexibility (compressive strength / flexural strength) |
≤3.0 |
|
Appearance |
Single packing,gray dry powder |
包装、贮存与运输: 三复合牛皮纸包装,25kg/袋,防潮、防雨,存于阴凉干燥处,保质期6个月;按非危险品运输。
Package, Storage and Transportation: 25kg/sack, kept in dry, cool place, 6 months’ quality guarantee period, deliver by the way of non-dangerous goods
使用方法:
Usage:
1、基层处理:粘贴的聚苯板表面应尽量平整、坚固、清洁,必要时可用粗砂纸适当打磨。聚苯板间应压紧,可能出现的板缝须用保温材料或发泡胶填充。
1. Base treatment: clean and level the surface of EPS board substrate. Distance between EPS board should be filled with thermal insulation materials
2、配制粘结砂浆:TDL013(外):水 =4:1 (重量比),使用电动搅拌器充分搅拌均匀,静置5-10分钟,再次搅拌即可使用,搅拌好的砂浆**好在2小时内用完,严禁将已凝固的砂浆二次搅拌再投入使用。
2. Mortar compounding: mix-ratio, TDL-013W: water = 4:1, fully mixed with electric mixer, standing for 5-10min, and mixed again; it is better to use up mixed mortar within 2 hours; no hardened mortar should be used.
3、用抹灰刀将抹面砂浆压于保温板上,然后将玻璃纤维网格布压入湿抹面砂浆中并找平。玻璃纤维网格布应搭接,搭接宽度不得少于10cm,网格布以似露非露为宜。抹面层厚度约为3-5mm。
3. Apply protection mortar on EPS board, then press into glass fiber mesh. The glass fiber mesh should be overlapped, the overlapped width be no less than 10cm, and the construction result of “seemly revealing non-exposure” is approximate. The protection mortar should be 3-5mm thick.
4、参考消耗量:4-5kg/m2。
4. Recommended quantity: 4-5kg/m2
注意事项:
Remark:
1、施工温度宜大于5℃ 以上,风力5级以下,避免雨天施工;在冬施情况下,应采用防冻型砂浆;
1. The favorable construction conditions: temperature >5℃, wind force<5, no construction no rainy days; frost-resistant mortar should be used in winter.
2、拌制好的砂浆应在2小时内用完 ,已凝固硬化的砂浆不得二次使用;
2. Mixed mortar should be used up within 2 hours; no hardened mortar should be used.
3、施工完毕24小时内,不得进行下一道工序的施工,同时应避免雨水冲刷、磕碰。
3. After construction, another step should start 24 hours later. It is necessary to avoid raining and bumping.