产品编号:TDL-063
Serial Number: TDL-063
用 途:适用于涂饰工程前,施涂于外墙外保温墙体,以找平为目的的基层表面处理材料。
Function: Leveling material for external thermal insulation system
产品介绍:
·良好的亲和性和粘结强度,可大大提高外墙涂料装饰质量和使用寿命
·耐候性强,良好的透汽性和抗裂性能
·和易性和保水性好,开放时间长,施工性能优异
·无毒、无害、环保型
Product Introduction:
· Strong affinity and adhesion strength
· Weatherproofing,crack resistance
· Good workability,water retentiveness,long open time
· No toxicity,no hazard,environmental friendliness
技术性能:
项目 |
性能 |
|
外观 |
单组分,干粉 |
|
施工性 |
刮涂无障碍 |
|
干燥时间(表干,h) |
≤5 |
|
打磨性 |
手工可打磨 |
|
吸水量,g/10min |
≤2 |
|
耐碱性(48h) |
无异常 |
|
耐水性(96h) |
无异常 |
|
低温贮存稳定性 |
-5℃冷冻4h无变化,刮涂无困难 |
|
粘结强度 |
标准状态,MPa |
≥0.60 |
冻融循环5次,MPa |
≥0.40 |
Technical Specifications:
Items |
Specification |
|
Appearance |
Single packing, dry powder |
|
Workability |
Easy to construct |
|
Drying time(h) |
≤5 |
|
Polishing |
Can be done manually |
|
Water absorption,g/10min |
≤2 |
|
Alkali resistance(48h) |
Normal |
|
Water resistance(96h) |
Normal |
|
Stability at low temperatures |
No change after freezing for 4 hours at -5℃, good workability |
|
Adhesive strength |
Standard,MPa |
≥0.60 |
5 freezing and thawing cycles’,MPa |
≥0.40 |
包装、贮存与运输: 三复合牛皮纸包装,25kg/袋,防潮、防雨,存于阴凉干燥处,保质期6个月;按非危险品运输。
Package, Storage and Transportation: 25kg/sack, kept in dry, cool place, 6 months’ quality guarantee period, deliver by the way of non-dangerous goods
使用方法:
Usage:
1、清理基层表面的油污和浮灰,并喷水湿润;
1. Clean and wet substrate;
2、TDL-063:水=1:0.5(重量比)使用电动搅拌器充分搅拌均匀,放置10分钟左右,再搅拌2分钟即可刮涂。拌和好的腻子应在2小时内用完。
2. Fully mix ( TDL-063:water = 1:0.5 ), 10minutes later, mix again and use; mixed putty should be used up within 2 hours;
3、刮涂腻子时手法要舒畅,**遍不宜刮的过厚,厚度在0.5mm-1mm之间为宜,待**遍腻子表干后,再刮第二遍腻子,一般两遍腻子成活;
3. Apply TDL flexible water-resistant putty 2 times: firstly, 0.5mm-1mm thick, then after dry, apply for the second time.
4、参考消耗量:1.5-2kg/m2。
4. Recommended quantity: 1.5-2kg/m2
注意事项:
Remark:
1、施工温度宜大于5℃ 以上,风力5级以下,避免雨天施工;在冬施情况下,应采用防冻型砂浆;
1. The favorable construction conditions: temperature >5℃, wind force<5, no construction no rainy days; frost-resistant mortar should be used in winter.
2、批刮腻子时不能漏底,应完全覆盖基层表面,批刮好的腻子表面干透后,可用细砂纸将不平处磨平,使其批刮均匀、无刮痕。
2. Fully cover the surface of substrate, after completely dry, polish with sand paper.
>> 了解更多信息